![](http://primarybook.net/images/bannerupbp01.gif)
Some Good people at Eurofab Technologies Ltd. are to bend it on a press brake.
www.eurofab.ie
There was a smaller test piece also marked up for the setup
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEgY4nKxHZPKiafAkO5ZxedoizDAmpKhmcvHN02MtSXOY-zJpHU731lt8wahStBI7QhqWHjRDpXcvObthvhK_hKGLVGFB8NxqLx6tZKgq-fskpzcxQpt5pAl8T0W_Rptm2nJ1W9_idk6kYTC/s320/25-10-08+02.jpg)
12th Feb we get a clear hour to do the bend as the factory is usually busy doing lots of repeat work.
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEgmBso2Ob0jkGzE-t1hmSo-4PDNkvUqd2iaK9lUnlCxsXWG-6kYJ858_dPCtbkzXqpMceTt3JvaaMkvxeO-Zd5qCTKG3y1PR8_1Prk55wPlkb2WdAwepiAAFk3eD3wrR_OG1DWwZPeD9BRb/s320/12-02-09+011.jpg)
First test piece 90 % correct.
We also did a piece only 2mm thick to get the bend radius correct.
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEikpqXD4kNm19Lcl_BvIUPk9pdPicCMWY4cBB_T1nqBx8vUwIKaEq1ZFaTK3SIJIOSAsUE4_auQq9ZgSreM3Phlpg5o21E6gMJQB31gc9D397JfnR3kWjVs-Qe8Ex2WXtZAKhyBDcw5vOwm/s320/12-02-09+013.jpg)
Final piece ready to get bent. I had the sheet marked at 22 degree intervals, we decided that more hits at 11 degrees would give a better shape.
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEgLVXBLumQD_hyjlFYNSq4elWw6NRkZDuc4HPj0NW5z-CcFcgWsxXKuzIlRJcujvCrw__7xDWNlkjsdQ5eqHFnkF52AUisgHkMg95C-AYrp0h31J2OFHIlceRmiKupAD8DJIhPOJH_uxu9p/s320/12-02-09+016.jpg)
All setup to go. 1 piece and 1 go. !!!
The Boys werent worried.....
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEiqbGslxOYdOALn7ouftXT7YZSdnXFMEjElTWa5NueehwUlzmAYYj9tJGhcgLRIRzP_PF02iqUmT0kGJvw1hRnj0vJ6-Pny8-R6XndUKaHLTgmjYPxhzv6HoJGebWzz2KOIku1Li0d4Bheh/s320/12-02-09+017.jpg)
Naturally the piece is 100% perfect. 270 mm Dia at the top and 110mm at the bottom.
Better than I expected.